This dataset describes the Shandong staged grinding and weak magnetic separation-reverse flotation process for magnetite. The process flow is as follows:
1. Staged Grinding
First Stage Grinding: The ore is crushed and enters the first stage grinding. The grinding fineness in the first stage is typically controlled at 60%~70% for particles of -0.074mm. The purpose of this stage is to liberate most of the iron minerals, facilitating preliminary enrichment by subsequent weak magnetic separation.
Second Stage Grinding: The slurry after the first stage grinding is classified by a hydrocyclone or spiral classifier. The coarse particles from the classification enter the second stage grinding. The grinding fineness requirement in the second stage is higher, typically controlled at 85%~90% or more for particles of -0.074mm. The purpose of this step is to further refine the ore, ensuring complete liberation of mineral particles and providing conditions for subsequent flotation. Item.
Three-stage grinding (optional): For some complex ores or high-requirement concentrate products, three-stage grinding can be performed. The grinding fineness in this stage can reach over 90% – 0.037mm, suitable for beneficiation needs requiring extremely fine mineral liberation.
Controlling the grinding fineness is crucial to flotation efficiency. Excessively coarse grinding leads to insufficient liberation of iron minerals and gangue minerals, affecting the concentrate recovery rate in subsequent flotation; while excessively fine grinding increases energy consumption and may cause over-refinement of the pulp, affecting pulp flowability and foam stability during flotation. Therefore, precise control of the grinding fineness is essential during staged grinding.
2. Weak Magnetic Separation
Process Description: The ground slurry enters a weak magnetic separator. Based on the magnetic characteristics of iron minerals, the separator adsorbs magnetic minerals onto the magnetic separator drum, while non-magnetic gangue minerals are discharged with the slurry. The purpose of this step is to initially remove gangue minerals, preparing for the subsequent reverse flotation process.
Product: The magnetic concentrate separated by magnetic separation enters the reverse flotation operation, while the unqualified slurry is sent to waste rock treatment.
3. Reverse Flotation
Technical Principle: Utilizing either cationic or anionic reverse flotation technology, gangue minerals are separated from iron minerals through a single roughing and cleaning process. Collectors and frothers are added during flotation; gangue minerals enter the flotation froth, while iron minerals remain in the pulp as concentrate.
Flotation Reagents: Depending on the ore properties, either cationic or anionic collectors can be used. Cationic collectors are typically used for ores rich in silicate minerals, while anionic collectors are suitable for more complex ores.
Results: The final product of reverse flotation is a high-grade iron concentrate, with an iron concentrate grade that can be increased to approximately 69%, while controlling the SiO₂ content below 4%. The iron content of the flotation tailings is typically between 10% and 12%.
4. Flotation froth treatment and regrinding
Regrinding process: After concentration, the flotation froth enters the regrinding stage. The grinding fineness is typically controlled to **<0.037mm, >90% of which are**, ensuring that the mineral particles are finely refined to achieve complete liberation.
Dewatering and scavenging: The regrinded slurry is treated in a dewatering tank, then undergoes multiple scavenging magnetic separations to further recover iron minerals. The scavenged concentrate is returned to the reverse flotation system for further separation.
5. Multiple scavenging and tailings disposal
Process description: The multiple scavenging process aims to further purify magnetic minerals through multi-stage magnetic separation, ultimately controlling the iron content in the tailings to approximately 10%~12%.
Product treatment: The scavenged concentrate is returned to the reverse flotation process for further refining, ensuring maximum iron mineral recovery. The tailings are discharged into a tailings pond for treatment.