Shanxi Province's steam coal is widely distributed in the Taiyuan Formation, Shanxi Formation, and Datong Formation. The Taiyuan and Shanxi Formations are mainly lean coal and anthracite, while the Datong Formation is primarily weakly caking coal. The Taiyuan Formation has an ash content of 12.62–28.52%, volatile matter of 6.5–14.79%, maximum thickness of the plastic layer at 0 mm, total sulfur in raw coal of 1.2–6.65%, and a net calorific value on an as-received basis (Qnet,ar) of 8136–8749 kcal/kg. The Shanxi Formation has an ash content of 8–35%, volatile matter in raw coal of 6.4–16.6%, maximum thickness of the plastic layer of 0–12 mm, and total sulfur in raw coal of 0.2–0. 92%, with a received basis net calorific value (Qnet,ar) of 8,350~8,577 kcal/kg. Datong Group raw coal has an ash content of 8.56~16.13%, refined coal volatile matter of 29.73~35.52%, maximum thickness of the vitrinite layer (G-index) of 0 mm, total sulfur content in raw coal of 0.49~1.93%, and a received basis net calorific value (Qnet,ar) of 7,705~7,946 kcal/kg.