This dataset describes the process of treating magnetite using staged grinding and weak magnetic separation-reverse flotation in Shanxi Province. The process flow is as follows:
1. Staged Grinding
First Stage Grinding: The ore is crushed and enters the first stage grinding. The grinding fineness in the first stage is typically controlled at -0.074mm, accounting for 60%–70%. The purpose of this stage is to liberate most of the iron minerals, facilitating preliminary enrichment by subsequent weak magnetic separation.
Second Stage Grinding: The slurry after the first stage grinding is classified by a hydrocyclone or spiral classifier. The coarse particles from the classification enter the second stage grinding. The grinding fineness requirement in the second stage is higher, typically controlled at -0.074mm, accounting for 85%–90% or more. The purpose of this step is to further refine the ore, ensuring complete liberation of mineral particles and providing conditions for subsequent flotation.
Third Stage Grinding (Optional): For some complex ores or high-requirement concentrate products, a third stage grinding process can also be performed. This stage of grinding can achieve a fineness of over 90% -0.037mm, suitable for beneficiation applications requiring extremely fine mineral liberation.
Controlling the grinding fineness is crucial for flotation efficiency. Excessively coarse grinding leads to insufficient liberation of iron minerals from gangue minerals, affecting the concentrate recovery rate in subsequent flotation; while excessively fine grinding increases energy consumption and may cause over-refinement of the pulp, affecting pulp flowability and foam stability during flotation. Therefore, precise control of the grinding fineness is essential during staged grinding.
2. Weak Magnetic Separation
Process Description: The ground pulp enters a weak magnetic separator. Based on the magnetic characteristics of iron minerals, the separator adsorbs magnetic minerals onto the magnetic separator drum, while non-magnetic gangue minerals are discharged with the pulp. The purpose of this step is to initially remove gangue minerals, preparing for the subsequent reverse flotation process.
Product: The magnetic concentrate separated by magnetic separation enters the reverse flotation operation, while unqualified pulp is sent to waste rock treatment.
3. Reverse Flotation
Technical Principle: Utilizing either cationic or anionic reverse flotation, gangue minerals are separated from iron minerals through a single roughing and cleaning process. Collectors and frothers are added during flotation; gangue minerals enter the flotation froth, while iron minerals remain in the pulp as concentrate.
Flotation Reagents: Depending on the ore properties, either cationic or anionic collectors can be used. Cationic collectors are typically used for ores rich in silicate minerals, while anionic collectors are suitable for more complex ores.
Results: The final product of reverse flotation is a high-grade iron concentrate, with an iron concentrate grade that can be increased to approximately 69%, while controlling the SiO₂ content below 4%. The iron content of the flotation tailings is typically 10%–12%.
4. Flotation Froth Treatment and Regrinding
Regrinding Process: After concentration, the flotation froth enters the regrinding stage. The grinding fineness is typically controlled to be above -0.037 mm (90%), ensuring that the mineral particles are finely refined to achieve complete liberation.
Dewatering and Scavenging: The regrinded slurry is treated in a dewatering tank, then undergoes multiple scavenging magnetic separation processes to further recover iron minerals. The scavenged concentrate is returned to the reverse flotation system for further separation.
5. Multiple Scavenging and Tailings Disposal
Process Description: The multiple scavenging process aims to further purify magnetic minerals through multi-stage magnetic separation, ultimately controlling the iron content in the tailings to approximately 10%–12%.
Product Processing: The scavenged concentrate is returned to the reverse flotation process for further refining, ensuring maximum iron mineral recovery. The tailings are discharged into a tailings pond for treatment.