The production of silicon-aluminum-iron alloys includes batching, smelting, casting, and finished product packaging processes. In the core smelting process, heat the cold furnace to about 600°C and start feeding. First, add aluminum ingots to the bottom of the furnace, melt them for about 8 minutes, then add ferrosilicon, and finally add scrap steel. When the raw materials in the furnace are free of granular materials, start stirring. The melting time of each furnace is controlled at about 35 minutes, and the melting temperature is 1000~1400°C.